Electrode |
銅-Copper(Cu+2) |
氰化物-Cyanide(CN-) |
氟-Flouride(F-) |
|
Mono/Combination |
CUO1501/CUO1502 |
CNO1501/CNO1502 |
FOO1501/FOO1502 |
|
Housing |
EPOXY/GLASS |
EPOXY/GLASS |
EPOXY/GLASS |
|
Slope |
27+/-2 |
57+/-2 |
57+/-2 |
|
Reproducibility |
±2% |
±2% |
±2% |
|
Temp Range |
0 to 80ºC |
0 to 80ºC |
0 to 80ºC |
|
Pressure Range |
0~30psi |
0~30psi |
0~30psi |
|
Response Time |
20seconds |
20seconds |
20seconds |
|
Concentration Range |
6.4~6350 |
0.13~260 |
0.2~saturated |
|
pH Range |
2 to 12 |
11 to 13 |
5 to 8 |
|
Interferences |
Ag+,Hg+2,high levelsof Cl-, |
S-2,I-,Br-,Cl |
OH- |
|
Electrode |
鎘-Cadmium(Cd+2) |
溴-Bromide(Br)- |
氯-Chloride(Cl-) |
|
Mono/Combination |
CD21501/CD21502 |
BRO1501/BRO1502 |
CLO1501/CLO1502 |
|
Housing |
EPOXY/GLASS |
EPOXY/GLASS |
EPOXY/GLASS |
|
Slope |
57+/-2 |
56+/-2 |
56+/-2 |
|
Reproducibility |
±2% |
±2% |
±2% |
|
Temp Range |
0 to 80ºC |
0 to 80ºC |
0 to 80ºC |
|
Pressure Range |
0~30psi |
0~70psi |
0~70psi |
|
Response Time |
30seconds |
30seconds |
30seconds |
|
Concentration Range |
0.2~11200 |
0.4~79900 |
1.8〜35500 |
|
pH Range |
2 to 12 |
2 to 14 |
2 to 12 |
|
Interferences |
Ag+,Hg+2,Cu+2,high levels of |
S-2,I,CN-,high levels of Cl- and NH3 |
S-2,I-,Br-,CN- |
|
Electrode |
碘-lodide(I-) |
鉛-Lead(Pb+2) |
銀-Silver Sulfide(Ag+/S-2) |
|
Mono/Combination |
I0O1501/IOO1502 |
PB21501/PB21502 |
AGS1501/AGS1502 |
|
Housing |
EPOXY/GLASS |
EPOXY/GLASS |
EPOXY/GLASS |
|
Slope |
57+/-2 |
25+/-2 |
157+/-2;27+/-2 |
|
Reproducibility |
±2% |
±2% |
±2% |
|
Temp Range |
0 to 80ºC |
0 to 80ºC |
0 to 80ºC |
|
Pressure Range |
0~70 psi |
0~70 psi |
0~70 psi |
|
Response Time |
30seconds |
30seconds |
30seconds |
|
Concentration Range |
6~127000 |
0.2~20700 |
Ag+=0.01〜107900 |
|
pH Range |
0 to 14 |
3 to 8 |
2 to 12 |
|
Interferences |
S-2,Br-,CN-,Cl-, |
Ag+,Hg+2,Cu+2, |
Hg2+,Hg+ |